Thermal Properties Metric English Comments
Crystallization Temperature 113 - 115 °C
235 - 239 °F
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
Crystallization Temperature 113 - 115 °C
235 - 239 °F
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer
Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f..
Crystallization Temperature 113 - 115 °C
235 - 239 °F
ISO 11357-3
Addcomp PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer
Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, ..
Crystallization Temperature 104 - 115 °C
219 - 239 °F
Average value: 110 °C Grade Count:7
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..