Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 124 °C | 255 °F | Peak, DSC; ASTM D3418 |
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF)
(Unverified Data**) High Melt Viscosity - Polymer for Non-Architectural Dispersion CoatingsInformation provided by Solvay Specialty Polymers. |
|||
Crystallization Temperature | 124 - 130 °C | 255 - 266 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF) Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Prope.. |
|||
Crystallization Temperature | 124 °C | 255 °F | Peak; ASTM D3418 |