Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Solvay Specialty Polymers
Trade Name Solef®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Properties: Heat of Fusion - ASTM D3418 38.0 to 48.0 J/g; Thermal Stability - TGA > 375 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.75 - 1.78 g/cc
0.0632 - 0.0643 lb/in³
ISO 1183
Water Absorption <= 0.20 %

@Time 86400 sec
<= 0.20 %

@Time 24.0 hour
ISO 62
Melt Flow <= 3.0 g/10 min
<= 3.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 1.00 - 1.50 GPa
145 - 218 ksi
1.0 mm/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point 160 - 168 °C
320 - 334 °F
DSC
Crystallization Temperature 124 - 130 °C
255 - 266 °F
Peak; ASTM D3418
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
DSC
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America