Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 330 - 380 °C | 626 - 716 °F | |
Chengdu Polyster PPHA p-Hydroxybenzoic Acid Polymer PPHA is difficult to manufacture and brittle as well as low mechanical strength, its compounds have a higher mechanical strength and can be injection moulded. It can work without oil and its perform.. |