Polymer Property : Crystallization Temperature = 78.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 26.0 °C
78.8 °F
ExxonMobil Method
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin
Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Crystallization Temperature 26.0 °C
78.8 °F
DSC, 10°C/min (peak); DuPont Test
Dow Engage® ENR 7447.00 Ethylene-Butene Copolymer
Description: ENR 7447.00 is a high flow, low density ethylene-butene copolymer designed for use in combination with our other elastomers to provide tailored solutions in polymer modification applica..