Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
Dow Corning MOLYKOTE® 1122 CHAIN AND OPEN GEAR GREASE Lubricating chains, gear drives, worm gears, slow-moving bearings. Resists water, steam and high temperatures; contains MoS2 for high loads and low speeds. Thick, black, tacky synthetic grease con.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application Temperature |
Chesterton 752 Cold Galvanizing Compound Description: Chesterton® 752 Cold Galvanizing Compound functions both as a zinc rich primer or final coating for ferrous metals and their welds exposed to atmospheric or corrosive conditions. The p.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 253 Silicone Splicing Tape 3M™ Sealing Splicing Tape 253 is a single-coated paper tape with a modified poly liner implemented as a second liner on the FACE SIDE of the tape. This second liner is added to help ensure roll qua.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7046 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 8620Cv2 ES Changeable Graphic Film with Comply™ v2 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M FP024408 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products FP024402 and FP024408 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra remova.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ 1000-57 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M ScotchCal™ 3690E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M ScotchCal™ 3698E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-17 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-193 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-273 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-89 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-12 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-120 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-15 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-176 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | flat surfaces without rivets |
3M Scotchlite™ 680-14 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Curves or corrugations with rivets |
3M Controltac™ IJ180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M FIP 1-Step Fire Barrier Rated Foam 3M Fire Barrier Rated Foam (FIP 1-Step), is a smoke, sound, and firestopping foam for wall and floor penetrations. Premium two-part, easy-to-handle formulations. Expands up to five times during inst.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ 1000-14 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ 3650-12 Graphic Film 2-mil opaque film; Available in white, black and transparent; Pressure-sensitive adhesive; Resists gasoline vapors and occasional petroleum spills; Permanent filmInformation provided by 3M |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-357 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7125-58 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-276 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | |
3M Scotchcal™ ElectroCut™ 7725-307 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Minimum Service Temperature, Air | 10.0 °C | 50.0 °F | Application |
3M 7940 Aluminum Foil Label Material 3M™Aluminum Foil Label Materials are durable, thin gauge, 1145 H19 aluminum designed to meet a wide range of difficult nameplate application requirements. 3M™Aluminum Foil Label Materials 7800, 78.. |