Thermal Properties Metric English Comments
Minimum Service Temperature, Air -90.0 °C
-130 °F
Recommended
Nye Lubricants UniFlor 8950 (497) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -90.0 °C
-130 °F
Recommended
Nye Lubricants UniFlor 8951 (897-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -90.0 °C
-130 °F
Recommended
Nye Lubricants UniFlor 8951R (897RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -90.0 °C
-130 °F
Precision Polymer Engineering S50E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci..
Minimum Service Temperature, Air -90.0 °C
-130 °F
Non-brittle after 3 minutes
Precision Polymer Engineering S50E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci..
Minimum Service Temperature, Air -90.0 °C
-130 °F
Precision Polymer Engineering S60E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 55-65 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci..
Minimum Service Temperature, Air -90.0 °C
-130 °F
Non-brittle after 3 minutes
Precision Polymer Engineering S60E Silicone Rubber
Red iron oxide filled, Phenyl Silicone Rubber, 55-65 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Speci..
Minimum Service Temperature, Air -90.0 °C
-130 °F
Components made from product
P & P Technology Silicone Sponge
The thermal stability of silicone rubber is probably its most important asset. Components made from these rubbers are affected only to a small extent by extremes of temperature, ranging from –90°C..