Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8180 (479) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8182R (837RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants UniFlor 8190 (483) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Polikim High Density Polyethylene (HDPE) High density polyethylene is preferred when resistance to chemicals and weather is the priority. As it can be supplied in large dimensions and can be welded, its use in construction of tanks and was.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Temperature at which stiffness does not exceed 70 Mpa |
Precision Polymer Engineering N60M Nitrile Rubber Nitrile Butadiene Rubber (NBR) 55-65 °IRHD. Medium acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet specification BS2751 BA60. Also meets obsolescent specification BS3.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Temperature at which modulus shall not exceed 70 Mpa |
Precision Polymer Engineering N70J Nitrile Rubber Peroxide cured Nitrile Butadiene Rubber (NBR), 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. To meet DTD 5594A standard for resistance to mineral oils.Applications: Excellent resistance i.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | ASTM D2137, Non-brittle after 3 minutes |
Precision Polymer Engineering V72H Fluoroelastomer Compound Fluoroelastomer Rubber, 65-75 °IRHD. FDA grade. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admi.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Precision Polymer Engineering Z95X Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 85-95 °IRHD. Medium acrylonitrile content (ACN = 36%). ASTM designation = HNBR.Applications: Gas blister resistant compound designed for use in applica.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Butyl Rubber (IIR, CIIR, BIIR) Butyl rubber is a copolymer of isoprene (minor) and isobutylene. Chlorobutyl (CIIR) and Bromobutyl (BIIR) contains 1.2% of the halogen. The halogen addition changes the cure characteristics and ca.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V75BR Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V90BR Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
GrafTech eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucobit® 1221 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit Simriz® 482 Low Temperature FFKT Perfluoroelastomer Compound Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of .. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Freudenberg Simrit V75 Standard Fluoroelastomer Excellent resistance to petroleum products and solvents. Very good high-temperature performance. Fluorocarbon elastomers make up the most widely used seals in the semiconductor industry. Avoid polar.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Gehman T100 |
Zeon Chemicals HyTemp® AR22 AR Super ACM Polyacrylate Elastomer Monomer composition is optimized for improved tensile strength and oil resistance over traditional acrylates. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg B939 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg Commercial Neoprene® C798 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg R608 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Chesterton 610 HT Synthetic Lubricating Fluid Description: Chesterton® 610 HT Synthetic Lubrication Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from -25°C (-15°F) for those over.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Chesterton 610 MT Plus Synthetic Lubricating Fluid Description: Chesterton® 610 MT Plus Synthetic Lubricating Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from 25°C (-15°F) to those o.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Chesterton 610 Synthetic Lubricating Fluid Description: Chesterton® 610 Synthetic Lubrication Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from -25°C (-15°F) for those over 27.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Dow Corning MOLYKOTE® G-0102 Heavy duty bearing grease for applications in presence of waterInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
ChevronTexaco NLGI 0 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | JIS-K-6723 |
Denka VINYKON M2510 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | JIS-K-6723 |
Denka VINYKON W5120 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | Recommended |
Nye Lubricants 865 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg R660 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -25.0 °C | -13.0 °F | |
Trelleborg Z600 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |