Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -200 - -26.1 °C | -328 - -15.0 °F | Average value: -134 °C Grade Count:13 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |