Thermal Properties Metric English Comments
Minimum Service Temperature, Air -47.8 °C
-54.0 °F
Arlon 920-410C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape  (discontinued **)
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu..
Minimum Service Temperature, Air -47.8 °C
-54.0 °F
Arlon 920-05B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular 0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Sel..
Minimum Service Temperature, Air -47.8 °C
-54.0 °F
Arlon 920-05C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular .0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Se..
Minimum Service Temperature, Air -47.8 °C
-54.0 °F
Arlon 920-10B##-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu..