Material Notes:
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fusing silicone tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length in yards.Arlon STD Certificate of Compliance for commercial applications will be provided with each order.Product is designed to meet the FAR 25.853 App.F, P.1,.AiiArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.Performance Advantages:Resists moisture, oxygen, and ozone to assure continuous high insulation values.Conforms smoothly when wrapped around complex forms.Bonds to itself at room temperature within 24 hours.Remains non-tacky to the touch and does not adhere to other surfaces, or substrates.Insulates with single wrap, thereby reducing labor time and cost.Dampens vibration and resists heat and mechanical shock as well as corona.Inherently flame resistant and when burned forms a non-conductive ash.SA & SB MOX-Tapes® provide a uniform thickness even around sharp edges. Fiberglass fabric, encapsulated inside the silicone rubber, prevents wicking and maintains high insulation resistance under high humidity conditions. These controlled stretch tapes provide a uniform insulation barrier.All tapes are protected by a special interleaved liner.Applications:Mechanical:Protection of coils from vibration.Vibration fixture, anti-scratch, and clamping pads.Harness wrapping and wire bundling, including for high temperature applications.Applied to rollers for protection and traction.Plant maintenance.Superior, heavy duty repair tape for emergency insulating barrier.Electrical:Insulation of field armature and interpole coils in large motors.Insulation for splicing and terminating of wire and cable.Insulating and sealing electrical connections.Insulating coil leads and bus bar connections.Electromagnetic coil insulation.Motor connections.Overwrapping of deteriorated insulation in reclaimed motors.Environmental:On-board aviation and space applications.Underground cable splices.Insulating heated transfer lines.Insulating in radioactive environments.Masking agent utilized in manufacturing processes and powder coatings.Insulating, protecting, and sealing rigging hardware and power systems in marine applications.This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Water Absorption 1.0 %
1.0 %
Arlon SQA-TMS-016
Thickness 63.5 microns
2.50 mil
Polyethylene, Interleave
508 microns
20.0 mil
Overall; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 7.674 MPa
1113 psi
Silicone Property; Arlon SQA-TMS-009
Elongation at Break 462 %
462 %
Silicone Property; Arlon SQA-TMS-009
Peel Strength 0.596 kN/m
3.40 pli
Bond Strength; Arlon- SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 95.6 °C
204 °F
Minimum Service Temperature, Air -47.8 °C
-54.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 27.6 kV/mm
701 kV/in
Arlon- SQA-TMS-020
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Brown