Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -63.0 °C | -81.4 °F | Cured |
Parker Chomerics Tecknit® 72-00014 Silver-Filled Flexible Resin Caulking System Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide .. |