Thermal Properties Metric English Comments
Minimum Service Temperature, Air -56.0 °C
-68.8 °F
Non-brittle after 3 minutes
Precision Polymer Engineering N75L Nitrile Rubber
Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Ultra-Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000/SAE J200 line call-out: MBF710, B34, F19.Application..
Minimum Service Temperature, Air -56.0 °C
-68.8 °F
Brittleness Temperature
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..