Polymer Property : Minimum Service Temperature, Air = -75.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -75.0 °C
-103 °F
Recommended
Nye Lubricants UniFlor 8970 (498) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -75.0 °C
-103 °F
Recommended
Nye Lubricants UniFlor 8971 (898-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -75.0 °C
-103 °F
Recommended
Nye Lubricants UniFlor 8971R (898RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -75.0 °C
-103 °F
Recommended
Nye Lubricants UniFlor 8971S (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -75.0 °C
-103 °F
NextGen Adhesives M907-19 Medical Grade Epoxy Adhesive
Description: NGAC M907-19 is a medium viscosity and thixotropic adhesive system that is specifically formulated for medical device assembly applications.Advantages and Applications: Uses include lam..
Minimum Service Temperature, Air -75.0 °C
-103 °F
Resin Technology Group 1217 Oxy-Bond™ Two-Component Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Minimum Service Temperature, Air -75.0 - -55.0 °C
-103 - -67.0 °F
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Resists ozone and oxidizing chemicals, alkali, aromatic chlorinated solvents. Affected by brake fluid, ketones, and hydrazine.
Minimum Service Temperature, Air -75.0 °C
-103 °F
Continuous
Isoflon ECTFE Fluoropolymer
Fluoropolymer material specifications.Information provided by Isoflon.
Minimum Service Temperature, Air -75.0 °C
-103 °F
as heat transfer fluid
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Minimum Service Temperature, Air -75.0 °C
-103 °F
ATG s.r.l. PVMQ Silicone Rubber
Minimum Service Temperature, Air -75.0 °C
-103 °F
CENTROPLAST CENTROLEN PE-HD Polyethylene high density
This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor..
Minimum Service Temperature, Air -75.0 °C
-103 °F
temperature limit for flexibility
Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation
Tygon® Ultra Chemical Resistant Tubing offers a combination of chemical resistance, clarity and flexibility. Tygon® 2375 replaces 2075.Tygon® Ultra Chemical Resistant Tubing is virtually unaffec..