Fluorosilicone Rubber (FMQ, FVMQ, FSi)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fluorosilicone Rubber (FMQ, FVMQ, FSi).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resists ozone and oxidizing chemicals, alkali, aromatic chlorinated solvents. Affected by brake fluid, ketones, and hydrazine.
Mechanical Properties Metric English Comments
Hardness, Shore A 25 - 90
25 - 90
Depends on compounding
Tensile Strength, Ultimate 8.60 MPa
1250 psi
Compounded Tire
Elongation at Break 100 - 400 %
100 - 400 %
Compression Set 3.0 %
3.0 %
Thermal Properties Metric English Comments
CTE, linear 810 µm/m-°C

@Temperature 20.0 °C
450 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -75.0 - -55.0 °C
-103 - -67.0 °F