Polymer Property : Minimum Service Temperature, Air = 149 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 149 °C
300 °F
Monmouth Rubber & Plastics Durafoamâ„¢ C41 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Minimum Service Temperature, Air 149 °C
300 °F
Monmouth Rubber & Plastics Durafoamâ„¢ C42 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Minimum Service Temperature, Air 149 °C
300 °F
Monmouth Rubber & Plastics Durafoamâ„¢ C43 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Minimum Service Temperature, Air 149 °C
300 °F
Monmouth Rubber & Plastics Durafoamâ„¢ C44 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Minimum Service Temperature, Air 149 °C
300 °F
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Minimum Service Temperature, Air 149 °C
300 °F
Monmouth Rubber & Plastics Durafoamâ„¢ P493SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Minimum Service Temperature, Air 149 °C
300 °F
Monmouth Rubber & Plastics Durafoamâ„¢ P497SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Minimum Service Temperature, Air 149 °C
300 °F
Lower limit of working range
Heatbath/Park Low Temperature Draw Salt Quenching and Tempering Salt
A eutectic mixture offering the lowest melting point and a wide working range. Formulated per MIL-S-10699-B, Class 1 (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical...
Minimum Service Temperature, Air 149 °C
300 °F
Lower limit of working range
Heatbath/Park Scale Kleen 1259 Descaling Salt
A highly alkaline and oxidizing salt bath used specifically as a low temperature bath for descaling titanium and titanium alloys.Information provided by Heatbath Corporation - Park Metallurgical.
Minimum Service Temperature, Air 149 °C
300 °F
Lower limit of working range
Heatbath/Park Thermo-Quench Oil
A "hot" or "marquenching" oil offering excellent thermal stability, high flash point and fast quenching rate.Information provided by Heatbath Corporation - Park Metallurgical.
Minimum Service Temperature, Air 149 °C
300 °F
Lower limit of working range
Heatbath/Park Thermo-Quench Quenching and Tempering Salt
Most widely used quench salt for more than a decade. This eutectic nitrate/nitrite mixture is highly recommended for the interrupted or isothermal quenching of austenitized steels. Slightly higher,..
Minimum Service Temperature, Air 149 °C
300 °F
Lower limit of working range
Heatbath/Park Parcure 275 Rubber Cure Salt
Nitrate/Nitrite Salt. An eutectic mixture offering the lowest possible melting point and the widest working range. (275 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
Minimum Service Temperature, Air 149 °C
300 °F
Lower limit of working range
Heatbath/Park Partherm 290 Heat Transfer Salt
The most widely used heat transfer salt. It is an eutectic mixture with a low melt point and a wide working range. (290 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical.
Copyright © lookpolymers.com All Rights Reserved