Polymer Property : Minimum Service Temperature, Air = 284 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 140 °C
284 °F
Synergy Polymers Ultra Purge CE-E
Best with color changes and material changes. Cleans out barrels, nozzles, heads of extruders and accumulators of blow molding machines from carbon remnants, deposits and incrustations. Has double f..
Minimum Service Temperature, Air 140 °C
284 °F
Synergy Polymers Ultra Purge LOW-E
Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean..
Minimum Service Temperature, Air 140 °C
284 °F
3M 855 High Temperature Nylon Tape
3M™ High Temperature Nylon Tape 855 is a 2 mil nylon film tape with a non-silicone rubber adhesive that can be used in many composite bagging operations or to help remove flashing after composite b..
Minimum Service Temperature, Air 140 °C
284 °F
3M 8555 High Temperature Nylon Tape
3M™ High Temperature Nylon Tape 8555 is a 5 mil film with a non-silicone rubber adhesive that can be used to help remove thick flash during composite bonding.Information provided by 3M