3M 855 High Temperature Nylon Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 855 High Temperature Nylon Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ High Temperature Nylon Tape 855 is a 2 mil nylon film tape with a non-silicone rubber adhesive that can be used in many composite bagging operations or to help remove flashing after composite bonding.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
ASTM D3752
Mechanical Properties Metric English Comments
Tensile Strength at Break 66.7 MPa
9670 psi
ASTM D3759
Elongation at Break 470 %
470 %
ASTM D3759
Peel Strength 0.60259 kN/m
3.4375 pli
Adhesion to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air 140 °C
284 °F
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Translucent cream color