Thermal Properties Metric English Comments
Minimum Service Temperature, Air 510 °C
950 °F
Lower limit of working range
Heatbath/Park #90 Casing Salt for Liquid Nitriding
An economical cyanide base salt which produces hard wear resistance properties for high speed tool steels in low dragout and/or low production use. It will maintain optimum operating characteristic..
Minimum Service Temperature, Air 510 °C
950 °F
Lower limit of working range
Heatbath/Park #90 Casing High Speed Hardening Salt
An economical cyanide base salt which produces hard wear resistance properties for high speed tool steels in low dragout and/or low production use. It will maintain optimum operating characteristic..