Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 510 °C | 950 °F | Lower limit of working range |
Heatbath/Park #90 Casing Salt for Liquid Nitriding An economical cyanide base salt which produces hard wear resistance properties for high speed tool steels in low dragout and/or low production use. It will maintain optimum operating characteristic.. |
|||
Minimum Service Temperature, Air | 510 °C | 950 °F | Lower limit of working range |
Heatbath/Park #90 Casing High Speed Hardening Salt An economical cyanide base salt which produces hard wear resistance properties for high speed tool steels in low dragout and/or low production use. It will maintain optimum operating characteristic.. |