Thermal Properties Metric English Comments
Minimum Service Temperature, Air 25.0 °C
77.0 °F
operating temp at 20 cPs
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid
Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and..
Minimum Service Temperature, Air 25.0 °C
77.0 °F
as heat transfer fluid
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..