Material Notes:
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature ranges, are available. Uses include heat transfer, electronic reliability testing, vapor phase soldering, solvents, and acid spill mitigation.
Physical Properties Metric English Comments
Density 1.85 g/cc

@Temperature 25.0 °C
0.0668 lb/in³

@Temperature 77.0 °F
Solubility of Water 0.0014 %
0.0014 %
Kinematic Viscosity 11.7 cSt

@Temperature 25.0 °C
11.7 cSt

@Temperature 77.0 °F
Molecular Weight 1550 g/mol
1550 g/mol
average
Vapor Pressure 0.00000400 bar

@Temperature 25.0 °C
0.00300 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 62.8 J/g

@Temperature 270 °C
27.0 BTU/lb

@Temperature 518 °F
at boiling point
CTE, linear 367 µm/m-°C
204 µin/in-°F
converted from volumetric expansion of 0.0011 cm<sup>3</sup>/cm<sup>3</sup>-°C
Specific Heat Capacity 0.960 J/g-°C
0.229 BTU/lb-°F
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Boiling Point 270 °C
518 °F
Maximum Service Temperature, Air 270 °C
518 °F
as heat transfer fluid
Minimum Service Temperature, Air 25.0 °C
77.0 °F
as heat transfer fluid
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+15 ohm-cm
6.00e+15 ohm-cm
Dielectric Constant 1.94

@Frequency 1000 Hz
1.94

@Frequency 1000 Hz
Dielectric Strength 15.7 kV/mm
399 kV/in
2.54 mm gap
Dissipation Factor 0.00020

@Frequency 1000 Hz
0.00020

@Frequency 1000 Hz
Descriptive Properties Value Comments
Appearance Clear and odorless
Solubility of Air (cm³ gas / 100 cm³ liquid) 26