Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 52.7 J/g | 22.7 BTU/lb | 80°C to end of melting; ASTM D3418 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers. |