Polymer Property : Heat of Fusion = 52.7 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 52.7 J/g
22.7 BTU/lb
80°C to end of melting; ASTM D3418
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers.