Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 66.0 J/g | 28.4 BTU/lb | 80°C to end of melting |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |