Thermal Properties Metric English Comments
Heat of Fusion 66.0 J/g
28.4 BTU/lb
80°C to end of melting
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer  (discontinued **)
Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..