Thermal Properties Metric English Comments
Heat of Fusion 53.0 - 60.0 J/g
22.8 - 25.8 BTU/lb
Crystallization Heat; ASTM D3418
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Heat of Fusion 53.0 - 60.0 J/g
22.8 - 25.8 BTU/lb
ASTM D3418
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Heat of Fusion 53.0 - 60.0 J/g
22.8 - 25.8 BTU/lb
Crystallization Heat; ASTM D3418
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Heat of Fusion 53.0 - 60.0 J/g
22.8 - 25.8 BTU/lb
ASTM D3418
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.