Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 54.0 - 60.0 J/g | 23.2 - 25.8 BTU/lb | Crystallization Heat; ASTM D3417 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 54.0 - 60.0 J/g | 23.2 - 25.8 BTU/lb | Crystallization Heat; ASTM D3417 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 50.0 - 60.0 J/g | 21.5 - 25.8 BTU/lb | Crystallization Heat; ASTM D3417 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 53.0 - 60.0 J/g | 22.8 - 25.8 BTU/lb | Crystallization Heat; ASTM D3418 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 53.0 - 60.0 J/g | 22.8 - 25.8 BTU/lb | ASTM D3418 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 53.0 - 60.0 J/g | 22.8 - 25.8 BTU/lb | Crystallization Heat; ASTM D3418 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 53.0 - 60.0 J/g | 22.8 - 25.8 BTU/lb | ASTM D3418 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |