Polymer Property : CTE, linear, Parallel to Flow = 14.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.7 µm/m-°C

@Temperature -30.0 - 30.0 °C
14.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DE002 PC
LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive.