Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 25.7 µm/m-°C @Temperature -30.0 - 30.0 °C |
14.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |