Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 16.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
9.00 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 3414R PC (Asia Pacific) 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C @Temperature -20.0 - 150 °C |
9.00 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2310R PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 1030 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 HS L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 HS UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 L N BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 L UV BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF30 RM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low Moisture AbsorptionAppearance: BlackTPCI# 9719102Information provided by T.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF33 HS L BK001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF40 A1 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: Lubricated, Low Shrinkage and Good Wear ResistanceAppearan.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF40 L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF40 TL20 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: PTFE Lubricant (20%) Features: LubricatedAppearance: BlackInformation provided.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF43 L BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection Mol.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF43 LE BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Low Ext.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M40 IG BK 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® R60 G33-L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorTPCI# 9208102Information.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6 GF30 RM BK Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: AntistaticAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA12 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT G/CF30 IM 15% Glass/Carbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInform.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS 0237 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS 0334 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b.. |
|||
CTE, linear, Parallel to Flow | 16.2 µm/m-°C | 9.00 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA12 1100 Tungsten Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Tungsten FillerInformation provided by TP Composites, Inc. |