Material Notes:
Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 2.37 g/cc
0.0856 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 103 MPa
15000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 12.4 GPa
1800 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 16.2 µm/m-°C
9.00 µin/in-°F
ASTM D696
Thermal Conductivity 1.73 W/m-K
12.0 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 280 °C
536 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 266 °C
510 °F
Unannealed; ASTM D648
UL RTI, Electrical 220 °C

@Thickness 1.50 mm
428 °F

@Thickness 0.0591 in
UL746
Flammability, UL94 V-0
V-0
5VB
5VB
Electrical Properties Metric English Comments
Volume Resistivity 10000 - 1.00e+6 ohm-cm
10000 - 1.00e+6 ohm-cm
ASTM D257