Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 35.1 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.5 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC
LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing.