CTE, linear, Parallel to Flow 2.00 - 3.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
1.11 - 1.67 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT
Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle..
CTE, linear, Parallel to Flow 2.00 - 3.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
1.11 - 1.67 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
CTE, linear, Parallel to Flow 2.00 - 3.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
1.11 - 1.67 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
CTE, linear, Parallel to Flow 2.00 - 3.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
1.11 - 1.67 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET
PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin..
CTE, linear, Parallel to Flow 2.00 - 3.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
1.11 - 1.67 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou..