Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 2.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
1.11 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66 LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 2.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
1.11 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DF005 PC LNP* Thermocomp* DF005 is a compound based on Polycarbonate containing 25% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 2.00 µm/m-°C @Temperature -40.0 - 150 °C |
1.11 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 2.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
1.11 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DE003M PC LNP* STAT-KON* DE003M is a compound based on Polycarbonate containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 2.00 - 3.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
1.11 - 1.67 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
CTE, linear, Parallel to Flow | 2.00 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
1.11 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
CTE, linear, Parallel to Flow | 2.00 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
1.11 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
CTE, linear, Parallel to Flow | 2.00 - 3.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
1.11 - 1.67 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
CTE, linear, Parallel to Flow | 2.00 - 3.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
1.11 - 1.67 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
CTE, linear, Parallel to Flow | 2.00 - 3.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
1.11 - 1.67 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
CTE, linear, Parallel to Flow | 2.00 - 3.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
1.11 - 1.67 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |
|||
CTE, linear, Parallel to Flow | 2.00 µm/m-°C | 1.11 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP AKV 35 LT H2.0 904040 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, black colored for laser transmission- welding (laser-transparent), good heat-ageing resistance |