Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FL900S PC (Europe-Africa-Middle East) Foamable Lexan* FL900S polycarbonate resin is an ideal choice for structural components where load bearing capability at elevated temperature is a key requirement. It exhibits outstanding inpact str.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-HGR24 Nylon 6-30% Glass Fiber and Glass Bead Reinforced (European Grade) (Dry)
(discontinued The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, DRY Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP QFN16 PA 6/10 LNP* LUBRICOMP* QFN16 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 5% MOS2. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
19.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON PX93058 PA 6 (Europe-Africa-Middle East) LNP*STATKON*PX93058 is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
19.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp DF008P PC (Asia Pacific) LNP* THERMOCOMP* DF008P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K223-HGM24 Nylon 6-30% Glass and Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
|
BASF Luranyl® KR 2403 G6 Polyphenylene Ether + Styrene-Butadiene Blend, 30% Glass Fiber Reinforced General-purpose grade with 30% glass fiber for parts requiring especially good resistance to heat deformation.Applications: parts for hot-water contact, pump housings, fan blades.Data was collected .. |
|||
CTE, linear, Parallel to Flow | 35.0 - 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
19.4 - 22.2 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TV4 264 SN PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East) LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges. |