Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp DF008P PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp DF008P PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* DF008P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0026 cm/cm

@Time 86400 sec
0.0026 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 142 MPa
20600 psi
ASTM D 638
148 MPa
21500 psi
ISO 527
Elongation at Break 2.3 %
2.3 %
ASTM D 638
2.3 %
2.3 %
ISO 527
Tensile Modulus 10.34 GPa
1500 ksi
50 mm/min; ASTM D 638
Flexural Strength 220 MPa
31900 psi
ISO 178
Flexural Modulus 18.0 GPa
2610 ksi
ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 35.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
19.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 37.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af