Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
47.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
47.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PX1005X PPE+HIPS (Europe-Africa-Middle East) Noryl PX1005X is an unfilled, low heat resistance, halogen free (according VDE/DIN 472 part 813) flame retardant material. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
47.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar DN003 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® R-T 60 Polycarbonate/ABS Blend Recycled grade in which carefully reclaimed old parts and production rejects and/or scrap from all processes of manufacturing or processing undergo material recycling. Slightly decreased impact stre.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 64 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 65 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® T45 PG Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 112 °Cfor electroplating applicationsPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® T50 BBS083 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Goo.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TS300 PA46 |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® KU 1-1446 Polycarbonate/ABS Blend Good cold impact strength and fuel resistance.Applications: Automotive industry (interior and body parts).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated fr.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 65 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Conditioned) Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistanc.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BESVO A FDA Nylon 11 (Conditioned) Designation ISO 1874-PA11,E,22-010Rigid grade for tubes and films extrusion in food applications. Available color: natural. Additive free.Good thermal and chemical resistance. Transparency. Barrier .. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BMN D Nylon 11 (Conditioned) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BMV Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,18-010Rigid grade for injection molding. Available color: natural. Free additive.High impact strength. Easy filling of the mold due to its well adapted melt viscosity. Lo.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | ISO 11359 |
BASF Ultramid® A34 01 PA66 (Dry) Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or .. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | ISO 11359 |
BASF Ultramid® B50L 01 PA6 (Dry) Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BMF Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,12-010Rigid grade for injection molding. Available color: natural. Additive free.Good melt viscosity. Outstanding ability to mold part with high length-thickness ratio an.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | ISO 11359 |
BASF Ultramid® B27 E 01 PA6 (Dry) Ultramid B27 E 01 is a low viscosity general-purpose, extrusion PA6 grade well suited for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German.. |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TE300 PA46 Heat Stabilized |
|||
CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Conditioned) Designation ISO 1874-PA11,E,24-010Rigid grade for extrusion blow molding. Available color: natural. Additive free.Very good impact strength. Well adapted melt strength. High chemical resistance.Food.. |