Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® HMG94MD ABS
Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature 20.0 °C
48.9 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 358-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature 20.0 °C
48.9 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® 446
Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12
LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant.
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature 20.0 °C
48.9 µin/in-°F

@Temperature 68.0 °F
ASTM data
Dow Prevail® 3150 ABS + Polyurethane
PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used ..
CTE, linear, Parallel to Flow 88.0 µm/m-°C
48.9 µin/in-°F
ISO 11359
BASF Ultramid® 8253 PA6 (Dry)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature 20.0 °C
48.9 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)  (discontinued **)
Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions..