Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 87624 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex NS0039XP PC+ABS (Europe-Africa-Middle East) LNP* FARADEX* NS0039XP is a compound based on PC/ABS resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Flame retardant.Thi.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® 18 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® 19 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® 27 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® F 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Apec® 1697 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 1881 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 2467 Polycarbonate ISO 7391-PC,MFLR,(,,)-18-9Global gradeFormerly Makrolon DP1-1870MVR (300 °C/1.2 kg) 19 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmLow viscosityUV stabilizedEasy r.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2665 MAS071 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 3158 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® DP1-1843* Polycarbonate ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® OD2015 Polycarbonate Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® Rx2635 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Med.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Altuglas® 84 L Acrylic-Styrene Copolymer ALTUGLAS 84 L is a new type of acrylic polymer produced by ATOHAAS which increases the range of material for injection molding applications. ALTUGLAS 84 L is a styrene methylmethacrylate copolymer s.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® LED2245 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeFormerly Makrolon DP1-1857MVR (300 °C/1.2 kg) 36 cm3/10 minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® Rx1452 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Oroglas® V 825 HID Acrylic, UV, Heat Resistant
(discontinued **) OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.Above 80°c, OROGLAS V 825 HID resin retains its original appearan.. |
|||
CTE, linear, Parallel to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® 27 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |