Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature -50.0 - 50.0 °C
3.89 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP JCL36 PES (Europe-Africa-Middle East)
LNP* LUBRICOMP* JCL36 is a compound based on Polyethersulfone resin containing Carbon Fiber, PTFE. Added features include : Internally Lubricated, Electrically Conductive.
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP OX91041 PPS - LINEAR (Europe-Africa-Middle East)
LNP* LUBRICOMP* OX91041 is a compound based on PPS Linear resin containing Carbon Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive.
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature -30.0 - 100 °C
3.89 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP
SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097..
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East)
Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature -50.0 - 50.0 °C
3.89 µin/in-°F

@Temperature -58.0 - 122 °F
1
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th..
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
3.89 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DD0009E PC
LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding.
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON DE006 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE006 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
3.89 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DE0069F PC
LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding.
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature -40.0 - 150 °C
3.89 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI
LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding.
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 85.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 216 PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert..
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature -40.0 - 150 °C
3.89 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP EC006APQ PEI
LNP* Thermocomp EC006APQ is a compound based on Polyetherimide containing 30% Carbon Fiber. Added features include: Electrically Conductive, High Flow.
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 85.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 85.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Solvay TECHNYL® A 216 NATURAL FA PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 Natural FA offers all of the primary properties of unreinf..
CTE, linear, Parallel to Flow 7.00 - 11.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
3.89 - 6.11 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT
Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic ..
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON RC008 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RC008 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.