Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 3.60 - 7.20 µm/m-°C
2.00 - 4.00 µin/in-°F
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber
Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab..
CTE, linear, Parallel to Flow 3.60 - 7.20 µm/m-°C
2.00 - 4.00 µin/in-°F
ASTM D696
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)  (Unverified Data**)
Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili..