Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester
Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -40.0 - 60.0 °C
39.4 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® RCY6013 PC+ABS (Asia Pacific)
Cycoloy* RCY6013 resin is an injection moldable high flow PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 @ 1.5 mm..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -40.0 - 60.0 °C
39.4 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® RCY6113 PC+ABS (Asia Pacific)
Cycoloy* RCY6113 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 5VB rating @ 2.0mm an..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -40.0 - 60.0 °C
39.4 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® RCY6214 PC+ABS (Asia Pacific)
Cycoloy* RCY6214 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1.5 mm. D..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
PolyOne Edgetek® XT X XT 1000 Natural Copolyester
Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP COLORCOMP D10006U PC
LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed.
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
39.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP DBL34E PC (Europe-Africa-Middle East)
LNP* LUBRICOMP DBL34E is a compound based on Polycarbonate resin containing Glass Bead, PTFE. Added features include: Easy Molding, Internally Lubricated.
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC
LNP LUBRICOMP* DL0029E is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant.
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
39.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXD164R PC (Europe-Africa-Middle East)
Transparent/translucent medium viscosity PC for light diffusion special effects, FDA compliant and mold release containing. The color package may affect performance.This data was supplied by SABIC-I..
CTE, linear, Parallel to Flow 71.0 µm/m-°C
39.4 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber
PA 66 injection molding grade, 30% glass fibers, UL 94V-2 at 0.75 mm , GWFI:960°C at 0.75 mm, GWIT: 775°C at 0,75 mm, halogen-freeApplication Examples: mixer insert for blenders, washing machi..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
39.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RBG16I PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RBG16I is a compound based on Nylon 66 resin containing Glass Bead, Graphite. Added features of this material include: High Impact.
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DX12411C PC
LNP* STAT-KON* DX12411C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer
LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled.
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature 20.0 °C
39.4 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 555 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP D7001IXH PC
LNP* THERMOCOMP* D7001IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare ap..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
39.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP NX11302 PC+ABS (Asia Pacific)
This is a PC/ABS compound with colorable, good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature 20.0 °C
39.4 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 213 ABS, General Purpose
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp WB008 PBT
LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
39.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Bayblend® FR3005 HG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
CTE, linear, Parallel to Flow 71.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
39.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/2
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..