Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
CTE, linear, Parallel to Flow 60.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
CTE, linear, Parallel to Flow 60.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® KR 4350 PA6/6T (Dry)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
CTE, linear, Parallel to Flow 70.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT
Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit..
CTE, linear, Parallel to Flow 50.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry)
ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase..
CTE, linear, Parallel to Flow 50.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
CTE, linear, Parallel to Flow 70.0 - 80.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 44.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl FN215D PPE+HIPS (Europe-Africa-Middle East)
NORYL FN215 is a Noryl Engineering structural foam grade fulfilling a wide range of application requirement. Moulded with the recommended blowing agents, this material provides all the performance r..