Polymer Property : CTE, linear, Parallel to Flow = 83.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 83.0 µm/m-°C
46.1 µin/in-°F
ASTM D696
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880...
CTE, linear, Parallel to Flow 83.0 µm/m-°C

@Temperature 20.0 °C
46.1 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® Elite HH 1827
Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding
CTE, linear, Parallel to Flow 83.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66
LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
CTE, linear, Parallel to Flow 83.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP IB008 PA 6/12 (Europe-Africa-Middle East)
LNP* Thermocomp* IB008 is a compound based on Nylon 6/12 resin containing Glass Bead.
CTE, linear, Parallel to Flow 83.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal
LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead.
CTE, linear, Parallel to Flow 83.0 µm/m-°C

@Temperature -40.0 - 100 °C
46.1 µin/in-°F

@Temperature -40.0 - 212 °F
ASTM E831
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
CTE, linear, Parallel to Flow 83.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP KFI12 Acetal Copolymer
LNP LUBRICOMP* KFI12 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant.
CTE, linear, Parallel to Flow 83.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66
LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant.