Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
51.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP AI001XXH ABS
LNP* Lubricomp* AI001XXH is a compound based on ABS containing 2% Silicone. Characteristics of this grade are: Healthcare and Internally Lubricated.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
Eastman Eastapak 9921W PET  (discontinued **)
Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® LGA-SF  (discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® 648
Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP MG004 PP (Europe-Africa-Middle East)
LNP* Lubricomp* MG004 is a compound based on Polypropylene resin containing Graphite Powder.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RL004 is a compound based on Nylon 66 resin containing PTFE.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON MX01767C PP
LNP* STAT-KON* MX01767C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON MX10301C PP
LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 2610 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 9010 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ 9450P ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
51.1 µin/in-°F

@Temperature 73.4 - 131 °F
ASTM E 831
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature 20.0 °C
51.1 µin/in-°F

@Temperature 68.0 °F
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Dry)
Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t..
CTE, linear, Parallel to Flow 92.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
51.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP Stat-kon MX01767C PP
LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB..