Polymer Property : Ring & Ball Softening Point = 107 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point 107 °C
225 °F
ASTM E28-99
3M Scotch-Weld™ 3794 Hi Tack PSA Bulk only Adhesive
Sprayable high tack PSA for bonding plastic, paper, metals, die-cut labelsInformation provided by 3M
Ring & Ball Softening Point 107 °C
225 °F
ASTM E28
Arkema Group EVATANE® 33-45 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-45 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-45 is stabilized with antioxidants. The High Vinyl Acetate co..
Ring & Ball Softening Point 107 °C
225 °F
ASTM E28-99
3M Scotch-Weld™ 6111HT Blue Bulk only Adhesive
Same as 6111 but has higher heat resistance and blue in colorInformation provided by 3M
Ring & Ball Softening Point 107 °C
225 °F
ASTM E28-99
3M Scotch-Weld™ 6111HT Tan Bulk only Adhesive
Same as 6111 but has higher heat resistanceInformation provided by 3M
Ring & Ball Softening Point 107 °C
225 °F
ASTM E28
Westlake Epolene® N-11 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-11 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..