Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 175 °C | 347 °F | ASTM E28 |
Arkema Group LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate LOTRYL® 29 MA 03 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 29 MA 03 is a polyme.. |