Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Transformation Temperature = -19.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature -19.0 °C
-2.20 °F
TR10; ASTM D1329
3M Dyneon™ FE 5520 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5520 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
Transformation Temperature -19.0 °C
-2.20 °F
TR10; ASTM D1329
3M Dyneon™ FE 5522 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5522 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
Copyright © lookpolymers.com All Rights Reserved