Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | -19.0 °C | -2.20 °F | TR10; ASTM D1329 |
3M Dyneon™ FE 5520 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5520 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
Transformation Temperature | -19.0 °C | -2.20 °F | TR10; ASTM D1329 |
3M Dyneon™ FE 5522 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5522 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |